MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC ASAHIKLIN AK-225T Hydrochlorofluorocarbon Solvent
Categories: Fluid; Solvent

Material Notes: AK-225T is a mixture of AK-225, ethanol, hydrocarbon and stabilizers. This blend was developed for those customers needing a more aggressive defluxer than AK_225AES. It has proven to be effective in preventing the formation of white residues and removing ionic contamination from printed circuit boards and other electronic devices. AK-225T has no flash point. However, since it is a blend, it could become flammable if greater than 15% by weight hydrocarbon concentrates in the boil sump of a degreaser or 20% by weight of the solvent evaporates. It is important to maintain the composition of AK_225T at or below this concentration by routine monitoring of the liquid in the water separator.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/cc
@Temperature 25.0 °C
Liquid
Solubility of Water 0.33 %25°C
Solubility in Water 0.062 %25°C
Viscosity 0.61 cP
@Temperature 25.0 °C
Vapor Pressure 0.570 bar
@Temperature 37.8 °C
Surface Tension 17.6 dynes/cm25°C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 47.2 cal/gb.p.
Specific Heat Capacity 1.34 J/g-°C
@Temperature 25.0 °C
Liquid
Melting Point -139 °C
Boiling Point 54.0 °C
 
Descriptive Properties
Flame Limit (vol% in air)5 to 10
Global Warming Potential (CO2=1, 100yr ITH)370
KB Value63
Relative Evaporation Rate (ether=100)72

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WAGC02 / 74558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.