Aromatic/aliphatic polyisocyanate based on toluylene diisocyanate/ hexamethylene diisocyanate. In combination with various Desmophen® grades or other suitable substances containing hydroxyl groups to formulate clear or pigmented, two-component polyurethane coatings characterized by rapid drying and good lightfastness. Properties / Applications: The rapid initial drying and early sandability are of particular advantage when formulating wood coatings. With just a few coats, high-bodied clear or pigmented finishes can be easily achieved. Information provided by Covestro |