ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applications include blow molded containers for packaging household and agricultural chemicals, particularly those that are strong stress crack-inducing reagents. Regulatory Status: L5332CP meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. This product is from the former Equistar product line. |