MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dymax 4-425 Glass Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes:
Ultra Fast™ Adhesives for Wire Harness, Strain Relief, Coil Coating and Terminating
Cost Effective
  • Ultra Light-Weld® UV/Visible adhesives set in as little as one second
  • On a material cost per application basis, Ultra Light-Weld adhesives are more cost effective than tape or cyanoacrylates
  • Ultra Light-Weld adhesives are easy to integrate on automatic winders (single and multi-spindle)

Improved Performance
  • Structural adhesion to all types of wire, wire cladding, bobbins, ferrites, ceramics and phenolics
  • Better durability than tapes, cyanoacrylates, solvent activated adhesives, hot melts or epoxies
  • Material has better thermal resistance than cyanoacrylates
  • Meets Mil Std 202 (Test methods 106E and 107G)

Fast, Two Step Processing
  • Dispense Adhesive
  • Cure in seconds with Dymax UV lightsource


Dymax 4-425 Glass Bonding Adhesive
Optically clear, durable, dishwasher safe; non-yellowing, flexible adhesion to many substrates, high strength, tough, resilient properties. Cure Type: UV Typical Use: Glass, ceramic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Cure Time <= 2.00 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Master Bond EP30QF Quartz filled, Two Part Epoxy System
Dow 733 GLASS & METAL SEALANT
Rogers Arlon Secure™ 48A50B020 0.020" Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell Encapsulation
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive

PDYYMAX03 / 34987

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.