MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ravago Manufacturing Americas Ravatuf™ 300X-1005A1 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: Mold in color/Partial paint
Features: Molding grade with good dimensional stability and low shrinkage (0.55%); Fully weatherable for automotive exterior/interior mold in color or partial paint; Ease of coloring by using PE or PP based color concentrates; Recyclability; Filler type: Talc, 21-23%

Availability: North America

Filler/Reinforcement: Talc, 22% Filler by Weight

Features: Good Colorability; Good Dimensional Stability; Good Weather Resistance; Low Shrinkage; Paintable; Recyclable Material

Uses: Automotive Exterior Parts; Automotive Interior Parts

Resin ID: PP+E/P-TD20

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
Elongation at Break 22 %22 %ASTM D638
Tensile Modulus  0.532 GPa
@Temperature 80.0 °C
77.2 ksi
@Temperature 176 °F
ASTM D638
 2.00 GPa
@Temperature 22.8 °C
290 ksi
@Temperature 73.0 °F
ASTM D638
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched (ISO)  2.73 kJ/m²
@Temperature -30.0 °C
1.30 ft-lb/in²
@Temperature -22.0 °F
Partial Break; ISO 180
 8.61 kJ/m²
@Temperature 0.000 °C
4.10 ft-lb/in²
@Temperature 32.0 °F
Partial Break; ISO 180
 29.4 kJ/m²
@Temperature 22.8 °C
14.0 ft-lb/in²
@Temperature 73.0 °F
Partial Break; ISO 180
Multi-axial Impact @ -30°C Total Energy  18.7 J
@Temperature -20.0 °C
13.8 ft-lb
@Temperature -4.00 °F
Ductile Failure; ISO 6603-2
 20.5 J
@Temperature 0.000 °C
15.1 ft-lb
@Temperature 32.0 °F
Ductile Failure; ISO 6603-2
 20.7 J
@Temperature -30.0 °C
15.3 ft-lb
@Temperature -22.0 °F
Ductile Failure; ISO 6603-2
 24.1 J
@Temperature -40.0 °C
17.8 ft-lb
@Temperature -40.0 °F
Ductile Failure; ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.2 - 45.0 µm/m-°C
@Temperature -30.0 - 100 °C
14.0 - 25.0 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM E228
CTE, linear, Transverse to Flow 54.0 - 73.8 µm/m-°C
@Temperature -30.0 - 100 °C
30.0 - 41.0 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM E228
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAVAGO41240 / 311933

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.