MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrene-Butadiene Copolymer

BK13 is an SBC developed specifically to have enhanced flow capabilities and improved stiffness over the KR01 grade. BK13 molded parts give excellent detail on rapid production cycles, and are easily processed by injection molding. This resin can be tinted or colored in a variety of transparent and opaque shades.

Applications: Major applications include displays, medical devices, overcaps, housings, and toys.

Processing Recommendations:
Injection Molding: Minimum melt temperature between 193-232°C necessary to permit mold fill. Minimum injection pressure required to fill the cavity. Maximum back pressure of 0.3 MPa. Drying: Generally, no need to dry resin.

Specification Data: FDA Regulation 21 CFR 177.1640; suitable for food contact. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50.

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccASTM D792
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76ASTM D2240
Tensile Strength, Yield 39.0 MPa2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 5.0 %2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 69.0 MPaTest specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 2.158 GPaTest specimens were injection molded by ASTM D1897; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °CASTM D648
Vicat Softening Point 89.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 93 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 193 - 232 °CInjection
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USP Class VI Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® KR03BR SBC

PCHEVK15 / 20276

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.