MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAMID® LX9039 NC Nylon 12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® LX9039 NC is an unmodified, medium viscosity polyamide 12 without stabilizers and processing aids. It is usually used only in special cases where the absence of any additives is desirable or the presence of processing aids interferes. VESTAMID® LX9039 NC is supplied as spherical granules, ready for processing in moisture-proof packaging. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Sustainable, Industry and Engineering, Sports and Lifestyle
Sustainability: Sustainable electricity
Delivery form: Pellets, Granules
Additives: Unfilled
Special Characteristics: Medium viscosity
Color: Natural color

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption 1.50 %1.50 %Sim to ISO 62
Moisture Absorption 0.700 %0.700 %Sim to ISO 62
Viscosity Number 180 cm³/g1.80 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.00800 cm/cm0.00800 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0110 cm/cm0.0110 in/inISO 294-4, 2577
Melt Flow 27.0 g/10 min
@Load 5.00 kg,
Temperature 240 °C
27.0 g/10 min
@Load 11.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 73.0
@Time 3.00 sec
73.0
@Time 0.000833 hour
ISO 7619-1
Tensile Strength at Break 50.0 MPa7250 psiISO 527
Tensile Strength 43.0 MPa6240 psiISO 527
Tensile Stress 32.0 MPa
@Strain 50.0 %
4640 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 43.0 MPa6240 psiISO 527
Elongation at Break 260 %260 %Nominal; ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 1.40 GPa203 ksiISO 527
Flexural Strength 46.0 MPa6670 psiat conv. Deflection; ISO 178
 58.0 MPa8410 psiISO 178
Flexural Modulus 1.42 GPa206 ksiISO 178
Flexural Strain at Break 7.00 %7.00 %at flexural strength; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 0.700 J/cm²
@Temperature -40.0 °C
3.33 ft-lb/in²
@Temperature -40.0 °F
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmcircular electrodes; IEC 62631-3-2
Dielectric Constant  3.00
@Frequency 1.00e+6 Hz
3.00
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 3.80
@Frequency 100 Hz
3.80
@Frequency 100 Hz
IEC 62631-2-1
 3.90
@Frequency 50.0 Hz
3.90
@Frequency 50.0 Hz
IEC 62631-2-1
Dielectric Strength 26.0 kV/mm660 kV/inAC, S20/P50; Sim. To IEC 60243-1
Dissipation Factor  0.0323
@Frequency 1.00e+6 Hz
0.0323
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.0500
@Frequency 100 Hz
0.0500
@Frequency 100 Hz
IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 150 µm/m-°C
@Temperature 25.0 - 55.0 °C
83.3 µin/in-°F
@Temperature 77.0 - 131 °F
ISO 11359-1/-2
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
Vicat Softening Point  138 °C
@Load 5.10 kg
280 °F
@Load 11.2 lb
50 K/h; ISO 306
 173 °C
@Load 1.02 kg
343 °F
@Load 2.25 lb
50 K/h; ISO 306
Glass Transition Temp, Tg 39.0 °C102 °FISO 11357-1/-2
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °F
Mold Temperature 60.0 °C140 °F
 
Descriptive Properties
Blue water consumption15.2 kgISO 14040, 14044
ColorNatural Color
Global Warming Potential1.6 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.6 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 5.6 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.2 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7925 / 325057

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.