MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis HK030U Polypropylene Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination with LGF concentrates on the injection molding process. The product is available in standard black 8229. Applications: HK030U has been developed especially for demanding applications in the automotive industry including front end carriers, noise shields, and under body shieldings.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Melt Flow 350 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 72.0 MPa132 N/10s; ISO 2039
Tensile Strength, Yield 33.0 MPa50mm/min; ISO 527-2
Elongation at Break 6.0 %50mm/min; ISO 527-2
Elongation at Yield 5.0 %50mm/min; ISO 527-2
Tensile Modulus 1550 MPa1mm/min; ISO 527-2
Flexural Strength 43.0 MPa
Flexural Modulus 1450 MPa2mm/min; ISO 178
Izod Impact, Notched (ISO) 1.60 kJ/m²
@Temperature -20.0 °C
ISO 180/1A
 1.80 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 11.0 kJ/m²ISO 179/1eU
 45.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 0.800 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 0.900 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 1.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 106 µm/m-°C
@Temperature -30.0 - 80.0 °C
Borealis Method
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °CISO 75-2
Vicat Softening Point 89.0 °C
@Load 5.10 kg
ISO 306
 151 °C
@Load 1.02 kg
ISO 306
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 - 80.0 °C
Melt Temperature 200 - 260 °Cmass temperature
Mold Temperature 30.0 - 50.0 °C
Injection Velocity 100 - 200 mm/sec
Hold Pressure 3.00 - 6.00 MPa
 
Descriptive Properties
Back Pressurelow to medium
Screw Speedlow to medium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total 3960 Polypropylene, Extrusion Grade
Borealis Daplen™ EE108U Polypropylene TPO Compound
Borealis ME266U Polypropylene Compound, Mineral Filled
Plastics Group Polifil® T-20 20% Talc-Reinforced Polypropylene
Total PPC 3120 MU5 Polypropylene, Heterophasic Copolymer, Automotive

PBOREA500 / 108759

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.