MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Semitron™ MDS 100 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: A modified PEEK with a remarkable combination of strength, stiffness, and stability. Specially developed for use in uncontrolled application environments where a high level of precision is required.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Water Absorption at Saturation 0.580 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 106ASTM D785
Tensile Strength 118 MPaISO 527-1/-2 (7)
Compressive Yield Strength 73.0 MPa
@Strain 1.00 %
ISO 604 (10)
 125 MPa
@Strain 2.00 %
ISO 604 (10)
Shear Strength 83.0 MPaASTM D732
Charpy Impact, Notched 2.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.37
@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.00700
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µin/in-°FASTM E-831 (TMA)
 20.0 µm/m-°C
@Temperature 23.0 - 100 °C
 20.0 µm/m-°C
@Temperature 23.0 - 150 °C
 21.0 µm/m-°C
@Temperature >=150 °C
Thermal Conductivity 0.250 W/m-K
 1.73 BTU-in/hr-ft²-°F
Melting Point 635 °FASTM D3418
Maximum Service Temperature, Air 480 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 410 °FASTM D648
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative
Mitsubishi Chemical Advanced Materials Semitron™ MP-370 Polyphenylsulfone
Mitsubishi Chemical Advanced Materials Semitron™ ESd 490HR PEEK Non-sloughing and low moisture absorption
Mitsubishi Chemical Advanced Materials Semitron™ ESd 520HR PTFE
Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 V PEI

P1SM34M / 85178

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.