MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay ALKAMULS® B Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Ethoxylated castor oil Emulsifier for oil and waxes in water based formulations. Emulsifier for fats, oils, fatty acids, waxes and solvents. Used as dispersant for pigments and iron powders. Dispersant for pigments and iron powders in magnetic coupling fluids. Paper dye-leveling

Identification: ETHOXYLATED OLEIC ACID

CAS: 61791-12-6

C.T.F.A./INCI Name : PEG-30 CASTOR OIL

Available in: Asia Pacific, Europe, Latin America and North America

Solubility in water at 25°C (2.0g in 10 mil): Miscible (RPG66)

Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.

Solubility in Ethanol 96° at 25°C (2.0g in 10 mil): Miscible

Applications: Emulsifier

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
pH 7.0 - 8.57.0 - 8.55% in water; RPG02
Iodine Absorption Number 28 - 3528 - 35[g l/100 g]; RPG13
 
Thermal PropertiesMetricEnglishComments
Pour Point 5.00 °C41.0 °F
Flash Point >= 100 °C>= 212 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 5.0<= 5.0
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 3.0 - 5.0 %3.0 - 5.0 %RPG16
 
Descriptive Properties
AppearanceLimpid Liquid amber yellow to clear brown
Cloud point70-75°C10% in BDG 25%, RPG08
CompositionActive content0.96
 Peroxides<2 meq O/Kg, statistical guaranty
HLB number11.8
Ionic ChargeNonionic
OdorSlight characteristicRPG31
Saponification number64-70 mg KOH/gRPG05

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD034 / 137264

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.