MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ITW Devcon® Flexane® Fast Cure Rubber Repair Liquid Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: A fast-curing, trowelable liquid urethane for repairing rubber equipment and filling expansion joints. Uses: Repair worn or damaged rubber equipment; form protective linings in equipment subject to wear, impact, abrasion, vibration, expansion, and contraction. Features; 400 ml reusable cartridge,Tack-free in 30 minutes, Fast, easy, no-mess dispensing, Thorough mixing of two components with automatic mix nozzle.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0377 lb/in³Cured
Solids Content 100 %
Viscosity 5800 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94ASTM D2240
Tensile Strength 3300 psiUrethanes; ASTM D412
Elongation at Break <= 450 %ASTM D412
Tear Strength 430 pliASTM D624
Taber Abrasion, mg/1000 Cycles 330
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 13.8 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °FWet
 180 °FDry
Shrinkage 0.18 %Linear During cure; ASTM D2566
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 24.0 °C
Functional cure
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 8.00 min
@Temperature 23.9 °C
 
Descriptive Properties
Chemical/Solvent Resistance1,1,1-Trichloroethane: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Aluminum Sulfate 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting Oil: Fair30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): poor30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric 36%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Isopropyl Alcohol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Potassium Hydroxide 40%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Xylene: poor30 day immersion at 75°F. Sample cured 7 days at RT
ColorGrayCured
Coverage106 in.²/lbCured. @ 1/4"
Mix Ratio by weight80 to 20Resin/Hardener
Specific Volume (in.³/lb)26.5Cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9186 / 239696

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.