MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 4462W Double Coated Polyethylene Foam Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces including polyethylene and polypropylene. 3M™ Double Coated Polyethylene Foam Tapes 4492G, 4492W, 4492B, 4496W and 4496B combine a conformable closed cell foam with a high strength acrylic adhesive that provides good initial tack and offers high ultimate adhesion to a wide variety of surfaces.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0960 g/cc
Thickness 0.800 mil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 0.415 MPaDynamic, 1 in.2 (6.45 cm2) overlap Jaw Speed 0.5 in./min (12.7 mm/min.); ASTM D-897
Peel Strength 8.00 pli90° Angle Peel 12 in./min. Jaw Speed (308 mm/min.) 72 hour Dwell; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 49.0 °CLong Term
 70.0 °CShort Term
 
Descriptive Properties
Adhesive Type745
LinerClosed Cell Crosslinked Polyethylene Foam

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam
J6 Polymers JFOAM™ BX-190 Engineered Specialty Foam
J6 Polymers JFOAM™ A-204 Engineered Specialty Foam
Hong Kun Group Lycopene Pharmaceutical Intermediate
ExxonMobil LD 503.LN Foams and Compounding Resin

PMM33904 / 168651

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.