Petrothene PP1711 is a nucleated polypropylene copolymer compound selected for use as fiber optic cable buffer tubes. This resin’s robust additive package provides enhanced thermal stability during processing and long term service at elevated temperature. Applications: Wire & CableInformation provided by LyondellBasell. |