MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
BASF Master Builders Solutions ChemRex® PRO 2000 Adhesive/Sealant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Typical applications of Pro 2000 adhesive/sealant include sealing around opening-doors, windows, air conditioners, skylights-in RV's, trailers and buses, bonding of vehicle trim and molding, waterproofing of roof and sidewall lap seams, bonding/sealing of joints constructed of prepainted metals, glass, aluminum and plastic composites, bonding of roof bows, waterproof and seal rivet seams, seal around corner and end moldings, glazing sealant on glass, aluminum, wood, concrete, fiberglass, and vinyl window systems, sealant for vinyl and aluminum.

Tack-free time is 25 minutes ± 3 minutes given the ASTM C 679 test method. Sag resistance is none given the ASTM C 2202 test method. Adhesion-in peel is 27 pli ± 3 pli given the ASTM C 794 test method. Bond durability is 25% total joint movement given the ASTM C 719 test method. Weathering after 500 hours indicates no change given the ASTM C 793 test method. No staining results from the ASTM 510 test method.

)

Information provided by ChemRex, Inc.

Product of former ChemRex, Inc. BASF launched the Master Builders Solutions brand on January 15, 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/ccASTM D1475
Brookfield Viscosity 1.40e+6 - 1.80e+6 cPBrookfield TF, 5 rpm, RT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM C661
Tensile Strength, Ultimate 2.07 - 2.41 MPaASTM D412
Elongation at Break 500 - 600 %ASTM D412

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1008 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round

PREX03 / 65562

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.