MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Durez® 5980 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez 5980 is a heat-reactive phenolic resin powder of the two-step type. Durez 5980 is recommended for use in the manufacture of friction elements.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 1.5 %Karl Fischer; DCT 4021A
Particle Mesh Size 200 MeshScreen Percent: < 3; DCT 4007A
 
Processing PropertiesOriginal ValueComments
Cure Time 67.5 sec
@Treatment Temp. 150 °C
DCT 4001A
 
Descriptive Properties
% Hexamine Content9DCT 4019A
Inclined Plate Flow (cold), 125°C, mm18.5DCT 4009B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Primacor® 5980I Ethylene Acrylic Acid (EAA)
Dow Primacor® 5990I Ethylene Acrylic Acid (EAA)
Dow Primacor® 5986 Ethylene acrylic acid copolymer
Dow Primacor® 3440 Ethylene Acrylic Acid (EAA)
Dow Primacor® 2912 Ethylene Acrylic Acid (EAA)

PSUMIT353 / 194158

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.