MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Leaded Copper, UNS C18700, H02 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing, Capacity for Being Cold Worked; Fair Suitability – Butt Weld; Poor Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Bending; Cold working; Drawing; Forging; Heading; Hot working; Impacting; Rolling; Swaging

Typical uses: Motor Parts; Connectors; Current Carrying Studs; Screw Machine Parts Requiring High Conductivity; Switch Parts; Current Carrying Bolts; Current Carrying Nuts

Applicable Specifications: Bar – ASTM B301/B301M; Rod - SAE J463, ASTM B301/B301M, SAE J461; Shapes – ASTM B301/B301M; Wires – ASTM B301/B301M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  290 MPa
@Thickness 25.4 mm
42000 psi
@Thickness 1.00 in
 296 MPa
@Thickness 6.35 mm
43000 psi
@Thickness 0.250 in
Tensile Strength, Yield  262 MPa
@Thickness 25.4 mm
38000 psi
@Thickness 1.00 in
0.5% Ext
 276 MPa
@Thickness 6.35 mm
40000 psi
@Thickness 0.250 in
0.5% Ext
Elongation at Break  18 %
@Thickness 6.35 mm
18 %
@Thickness 0.250 in
 25 %
@Thickness 25.4 mm
25 %
@Thickness 1.00 in
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 85 %85 %
Shear Strength  172 MPa
@Thickness 25.4 mm
25000 psi
@Thickness 1.00 in
 179 MPa
@Thickness 6.35 mm
26000 psi
@Thickness 0.250 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000179 ohm-cm0.00000179 ohm-cm96% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 31.4 W/m-K218 BTU-in/hr-ft²-°F
Melting Point 952.8 - 1080 °C1747 - 1976 °F
Solidus 952.8 °C1747 °F
Liquidus 1080 °C1976 °F
Annealing Point 427 - 649 °C800 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 760 - 871 °C1400 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.5 %>= 99.5 %
Lead, Pb 0.80 - 1.5 %0.80 - 1.5 %
 
Descriptive Properties
Cold Work (%)200.25 in
 201 in

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC18700x1 / 292857

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.