MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxies, Etc 20-2362 FR Flame Retardant Polyurethane Potting & Encapsulating Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: The 20-2362FR potting and encapsulating compound has been formulated to meet the stringent non-burning requirements of UL 94 V-0. 20-2362FR is listed with Underwriter’s Laboratory for passing UL 94 V-0. This system offers a unique combination of properties. 20-2362 is very low in viscosity, flame retardant, has a glass transition temperature of -72?C, and has low moisture permeability. This product forms a soft elastomer that will cushion and protect sensitive electronic components.

Features:

  • Flame Retardant - UL 94 V-0 listed
  • Low Viscosity
  • Low Durometer
  • Low Shrinkage & Exotherm
  • Excellent Moisture Resistance
  • Maintains Flexibility at Low Temperatures
  • RoHS and REACH compliant
Benefits:
  • May be used in applications requiring FR
  • Quick self-leveling around components
  • Low stress on components & vibration resistance
  • Will not damage components during cure
  • Will not absorb H2O and can be used in wet environments
  • Can be used in very cold environments
  • Finished products are export compliant

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccPolyol
 1.24 g/cc1.24 g/ccIsocyanate
Viscosity 315 cP315 cPCatalyst
 2500 cP2500 cPMixed
 7500 cP7500 cPResin
Storage Temperature 18.0 - 30.0 °C64.4 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090
Tensile Strength 2.76 MPa400 psi
Elongation at Break 40 %40 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+16 ohm-cm6.00e+16 ohm-cm
Surface Resistance 1.00e+16 ohm1.00e+16 ohm
Dielectric Constant 4.5
@Frequency 1000 Hz
4.5
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 228 µm/m-°C127 µin/in-°F
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg -72.0 °C-97.6 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 80.0 °C
1.00 hour
@Temperature 176 °F
 120 min
@Temperature 65.0 °C
2.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 20.0 min
@Load 0.100 kg
20.0 min
@Load 0.221 lb
 
Descriptive Properties
ColorBlack
Mix Ratio100:22by weight mixed (P:I)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX113 / 316790

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.