MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The combination of mineral and glass fibers result in a high performance, low warp and cost effective engineering thermoplastic. It exhibits high strength, good UV resistance, rigidity and good heat distortion temperatures. It has a relatively high resistance to creep under load. The heat stabilizer system extends its retention of properties at elevated temperatures. It has good chemical resistance to greases, oils and hydrocarbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccISO 1183
Melt Density 1.289 g/cc
@Temperature >=220 °C
ISO 1183
Water Absorption 0.90 %24 hour; ISO Test
 5.7 %ISO 62
Moisture Absorption at Equilibrium 1.6 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.0040 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM Test
Tensile Strength at Break 125 MPa0.2 in/min; ASTM Test
 51.0 MPa
@Temperature 120 °C
ISO Data
 51.0 MPa
@Temperature 120 °C
ASTM Test
 59.0 MPa
@Temperature 80.0 °C
ASTM Test
 59.0 MPa
@Temperature 80.0 °C
ISO Data
 178 MPa
@Temperature -40.0 °C
ASTM Test
 178 MPa
@Temperature -40.0 °C
ISO Data
Tensile Strength, Ultimate 115 MPa5mm/min; ISO 527
Elongation at Break 2.0 %5mm/min; ISO 527
 2.0 %0.2 in/min; ASTM Test
 3.0 %
@Temperature -40.0 °C
ASTM Test
 3.0 %
@Temperature -40.0 °C
ISO Data
 11 %
@Temperature 120 °C
ISO Data
 11 %
@Temperature 120 °C
ASTM Test
 13 %
@Temperature 80.0 °C
ASTM Test
 13 %
@Temperature 80.0 °C
ISO Data
Tensile Modulus 9200 MPa1mm/min; ISO 527
 2620 MPa
@Temperature 120 °C
ISO Data
 3090 MPa
@Temperature 80.0 °C
ISO Data
 10790 MPa
@Temperature -40.0 °C
ISO Data
Flexural Strength 178 MPaISO Data
 200 MPaASTM Test
Flexural Modulus 7200 MPaISO Data
 7580 MPaASTM Test
Izod Impact, Notched 0.550 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 6.00 kJ/m²ISO Test
 4.00 kJ/m²
@Temperature -40.0 °C
ISO Test
Charpy Impact Unnotched 4.60 J/cm²ISO 179
Charpy Impact, Notched 0.550 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
Specific Heat Capacity 2.028 J/g-°CMelt
Thermal Conductivity 0.250 W/m-KMelt
Melting Point 220 °C10 K/min
 220 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75
 202 °CASTM Test
Flammability, UL94 HB
 HB
@Thickness 3.00 mm
 
Descriptive Properties
ColorBK-106
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat
 X
 X
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Envalior Durethan® B 30 S 000000 Nylon 6 (PA6), Dry
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Dry)
Envalior Akulon® K222-D PA6, Dry, Low Viscosity
Envalior Akulon® K224-G6U (Dry) 33% Glass Reinforced Nylon 6 (North America)

PBASF9193 / 84957

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.