MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Special Metals INCONEL® Alloy MA 754
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A mechanically alloyed nickel-chromium alloy with oxide dispersion strengthening. Mechanical alloying, which involves high-energy milling of metal powders, is used to create a uniformly distributed, fine dispersoid of yttrium oxide in the alloy. The dispersoid, which is stable to the alloy's melting point, imparts exceptional high-temperature strength and creep resistance. The alloy's strength, corrosion resistance, and microstructural stability make it useful for gas-turbine vanes and other extreme-service applications. Standard product forms are round, flats, extruded section, plate, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: Nickel-Chromium Alloy; UNS N07754
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 950 MPaAnnealed
 730 MPa
@Temperature 550 °C
Annealed prior to test
Tensile Strength, Yield 570 MPaAnnealed
 500 MPa
@Temperature 550 °C
Annealed prior to test
Elongation at Break 20 %Annealed prior to test.
 18 %
@Temperature 550 °C
Annealed prior to test.
Rupture Strength 13600 psi
@Temperature 1090 °C,
Time 3.60e+6 sec
 14800 psi
@Temperature 1090 °C,
Time 360000 sec
 18700 psi
@Temperature 982 °C,
Time 3.60e+6 sec
 19700 psi
@Temperature 982 °C,
Time 360000 sec
 24000 psi
@Temperature 816 °C,
Time 3.60e+6 sec
 27000 psi
@Temperature 816 °C,
Time 360000 sec
 37200 psi
@Temperature 649 °C,
Time 3.60e+6 sec
 41200 psi
@Temperature 649 °C,
Time 360000 sec
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0001075 ohm-cm
Magnetic Permeability 1.001at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.2 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 14.26 W/m-K
Melting Point 1400 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.30 %
Carbon, C 0.050 %
Chromium, Cr 20 %
Iron, Fe 1.0 %
Nickel, Ni 78 %
Titanium, Ti 0.50 %
Y2O3 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 718
Special Metals INCONEL® Alloy 751
Special Metals INCONEL® Alloy X-750
Copper, Cu; Annealed
Special Metals INCONEL® Alloy 617

NINC37 / 17406

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.