MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HB Fuller Cyberbond ETM 44 Adhesive
Categories: Polymer; Adhesive

Material Notes: Profile: Threadlocking; medium strength, medium viscosity, thixotropic. Anaerobic adhesive for locking and sealing of threaded fasteners which can be disassembled with standard hand tools. ETM 44 is not classified as a hazardous mixture according to CLP. RoHS compliant.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Viscosity 400 - 800 cP
@Shear Rate 160 1/s
cone-plate
 3000 - 8000 cP
@Shear Rate 0.500 1/s
cone-plate
Storage Temperature 8.00 - 21.0 °C
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 10.0 - 18.0 MPaCompressive
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 30.0 secSet time, M10 brass bolt/nut
 24.0 hourFull Cure
Shelf Life 12.0 Month
 
Descriptive Properties
Adhesive strength10-18 NmSteel
 10-18 NmStainless steel V2A
 12-20 NmGalvanized steel
 12-20 NmBrass
Base compoundDimethacrylate
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL036 / 316827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.