MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zotefoams Plastazote® MP15FR Metallocene Polyethylene Foam, Flame Retardant
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Compliant with EC food contact regulations.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0150 g/ccNominal skin/skin; BS ISO 7214 1998
 0.0140 - 0.0180 g/ccsheet density
Cell Length 0.200 - 0.600 mm
 0.900 mmTypical Diameter
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 2610 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.353 MPaISO 7214 1998
Elongation at Break 146 %
Compressive Yield Strength 0.0180 MPa
@Strain 10 %
BS ISO 7214 1998
 0.0350 MPa
@Strain 25 %
BS ISO 7214 1998
 0.0620 MPa
@Strain 40 %
BS ISO 7214 1998
 0.0890 MPa
@Strain 50 %
BS ISO 7214 1998
Tear Strength 0.545 kN/mBS EN ISO 8067 1995
Compression Set 5.0 %
@Time 79200 sec,
Strain 25 %
24 hr recovery; BS ISO 7214 1998
 18 %
@Time 79200 sec,
Strain 25 %
0.5 hr recovery; BS ISO 7214 1998
 26.5 %
@Time 79200 sec,
Strain 50 %
24 hr recovery; BS ISO 7214 1998
 38 %
@Time 79200 sec,
Strain 50 %
0.5 hr recovery; BS ISO 7214 1998
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0390 W/m-Kmean temp of 10°C; ISO 8302 1991
Maximum Service Temperature, Air 95.0 °C
Minimum Service Temperature, Air -70.0 °C
Flammability Test 2.6
@Thickness 13.0 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 4.0
@Thickness 5.00 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 
Descriptive Properties
FlammabilityAutomotive: FMVSS.302 burn ratePass: > 3 mm thick
 Aviation: CAA8/2-2.2bComplies
 Construction: DIN4102 B1Pass: 6 to 20 mm thick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 6870 Polycarbonate
Zotefoams Plastazote® HL34 Polyethylene Foam
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam
Zotefoams Plastazote® LD18 Low Density Polyethylene Foam
Zotefoams Plastazote® HL79 Polyethylene Foam

PZOTEF937 / 150693

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.