MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chosun Refractories LW-20 Special Insulating Firebrick
Categories: Ceramic

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.500 g/cc>= 0.0181 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength <= 0.588 MPa<= 85.3 psiCold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity >= 0.174 W/m-K
@Temperature 350 °C
>= 1.21 BTU-in/hr-ft²-°F
@Temperature 662 °F
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 >= 1.0 %>= 1.0 %
 
Descriptive Properties
Main ApplicationsVarious Furnace inside lining
Temp.(°C) Reheating Shrinkage less than 0.5%1,200

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics Kaolite 1600 Super Lightweight Insulating Castables
Skamol Group V-1100 375 Vermiculite Insulating Slab
Pyrotek Wollite 50 Insulating Castable
NanoAmor 95%, OD: 20-30 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes
NanoAmor 95% 10-20 nm Aligned Multi-Walled Carbon Nanotubes

CCHOS086 / 124030

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.