MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Leaded Tin Bronze, UNS C92700, Copper Casting Alloy, M07 Temper, As Continuous Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Continuous Cast

Casting Characteristics: High – Effect of Section Size; Medium – Casting Yield, Fluidity, Gassing; Low - Drossing, Shrinkage in Solidification

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing

Typical uses: Lead Screw Nuts; Bearings; Bushings; Gears; Heavy Duty Bearings; Pump Impellers; Pump Pistons; Steam Fittings

Applicable Specifications: As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M, ASTM B505/B505M; As Sand Cast – Castings SAE J461, Castings SAE J462; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.77 g/cc0.317 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 77
@Load 500 kg
77
@Load 1100 lb
Tensile Strength >= 262 MPa>= 38000 psifor Standard
Tensile Strength, Yield >= 138 MPa>= 20000 psifor Standard, 0.5% Ext
Elongation at Break >= 8.0 %>= 8.0 %for Standard
Tensile Modulus 110 GPa16000 ksi
Machinability 45 %45 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000156 ohm-cm0.0000156 ohm-cm11% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 200 °C
10.0 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 3.92 W/m-K27.2 BTU-in/hr-ft²-°F
Melting Point 316 °C600 °FIncipient
 843 - 982 °C1550 - 1800 °F
Solidus 843 °C1550 °F
Liquidus 982 °C1800 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.25 %<= 0.25 %
Copper, Cu 86 - 89 %86 - 89 %
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb 1.0 - 2.5 %1.0 - 2.5 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.25 %<= 0.25 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Sulfur, S <= 0.050 %<= 0.050 %
Tin, Sn 9.0 - 11 %9.0 - 11 %
Zinc, Zn <= 0.70 %<= 0.70 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC92700x1 / 293213

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.