MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Clyrell EC 390T Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell EC390T is a high flow clarified polyolefin resin used in injection molding applications. Clyrell EC390T features a good impact resistance at room and sub-zero temperature, high gloss and good resistance to stress whitening. Clyrell EC390T is typically used in clear impact container, toys, house wares. Applications: Clear Containers, House wares, Sports, Leisure & Toys, TWIM Food Containers, TWIM Non-food Containers

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 45 g/10 min
@Load 2.16 kg,
Temperature 230 °C
45 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 50 %>= 50 %ISO 527-1,-2
Elongation at Yield 13 %13 %ISO 527-1,-2
Tensile Modulus 1.15 GPa167 ksiISO 527-1,-2
Charpy Impact, Notched  0.300 J/cm²
@Temperature -20.0 °C
1.43 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise, Notch A; ISO 179
 0.400 J/cm²
@Temperature 0.000 °C
1.90 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise, Notch A; ISO 179
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -50.0 °C<= -58.0 °FISO 6603-2
 
Optical PropertiesMetricEnglishComments
Haze 30 %
@Thickness 1.00 mm
30 %
@Thickness 0.0394 in
injection molded disc; ASTM D1003
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H65C-00 Polypropylene Homopolymer
Ineos H05H-01 Polypropylene Homopolymer
Ineos H02C-00 Polypropylene Homopolymer
Braskem D040A Homopolymer Polypropylene
Borealis BorPURE™ RG466MO Polypropylene, Transparent Random Copolymer

PEQT7092 / 218729

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.