MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pressure Seal 49770 Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Compound 49770 is a 75 durometer clear colored BioMedical enhanced tear resistant Silicone. It also meets the requirements of USP Class V & VI. This compound will meet or exceed the specifications listed and has the following physical properties: United States Pharmacopeia (USP), Class V & VI
European Pharmacopeia (EP) (Ph.Eur.)
EP - Volatile Matter
EP - Substances soluble in Hexane
21CFR177.2600
This Compound is RoHS Compliant

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575
Tensile Strength 7.481 MPa1085 psi
Elongation, Ultimate 649 %649 %
Tear Strength 39.4 kN/m225 pliDie B
Compression Set 76.2 %
@Treatment Temp. 177 °C,
Time 79200 sec
76.2 %
@Treatment Temp. 351 °F,
Time 22.0 hour
Plied
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL206 / 318416

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.