MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes:

Hexene Copolymer

Features:

  • Excellent stiffness
  • Excellent puncture
  • High strength and toughness

Additives:

  • Processing antioxidant
  • Polymer process aid
  • Antiblock (900 ppm)
  • Slip (450 ppm)

Applications:

  • Industrial packaging
  • Overwrap
  • High clarity shrink film

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

United States: NOVAPOL TF-Y534-IP resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.<

Data provided by the manufacturer.

Key Words: Medium Density Polyethylene; Polyhexene; Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.934 g/ccASTM D792
Thickness 1.00 mil
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 15.0 MPaASTM D882
Film Tensile Strength at Yield, TD 17.0 MPaASTM D882
Film Elongation at Break, MD 520 %ASTM D882
Film Elongation at Break, TD 760 %ASTM D882
Secant Modulus, MD 0.350 GPaASTM D882
Secant Modulus, TD 0.410 GPaASTM D882
Coefficient of Friction 0.38ASTM D1894
Elmendorf Tear Strength, MD 2.00 g/micronASTM D1922
Elmendorf Tear Strength, TD 21.0 g/micronASTM D1922
Dart Drop 2.80 g/micronF 50; ASTM D1709/A
Film Tensile Strength at Break, MD 44.0 MPaASTM D882
Film Tensile Strength at Break, TD 32.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %
@Thickness 0.0250 mm
ASTM D1003
Gloss 63 %45°; 1 mil; ASTM D1894
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE
NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin
NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin
Braskem HF3712 Extrusion Linear Low Density Polyethylene
LyondellBasell Petrothene® GA837091 Linear Medium Density Polyethylene

PEHN3W / 35653

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.