MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Unipetrol Ethylhexanol
Categories: Fluid; Solvent

Material Notes: 2-ethylhexanol is produced by propylene oxonation to n-butyraldehyde and by subsequent aldolization and hydrogenation. It is a transparent, colourless, flammable liquid of a characteristic odour, hardly water-soluble. 2-ethylhexanol is used for production of acrylic acid esters, softening agents for plastics and synthetic rubber, components of synthetic lubricants and further as a solvent of oils, greases, waxes and resins.

Information provided by Unipetrol RPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.831 - 0.834 g/cc
@Temperature 20.0 °C
0.0300 - 0.0301 lb/in³
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.030<= 0.030mg KOH/g
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Component Elements PropertiesMetricEnglishComments
Free Water <= 0.050 %<= 0.050 %
 
Descriptive Properties
Aldehydes and Ketones, max0.04
Unsaturated Compounds, max0.02

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUNIP103 / 82963

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.