MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silver Bromide, AgBr (Bromirite)
Categories: Ceramic; Halide; Other Engineering Material; Semiconductor

Key Words: Halide; Semiconductor
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.473 g/cc0.2339 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.52.5
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 12.412.4
Band Gap 2.5 eV2.5 eV
Electron Mobility, cm²/V-s 40004000
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 49.0 J/g21.1 BTU/lb
Specific Heat Capacity 0.270 J/g-°C0.0645 BTU/lb-°F
Melting Point 1297 °C2367 °FTransition 147°C
Heat of Formation 486 kJ/mol486 kJ/mol
 
Optical PropertiesMetricEnglishComments
Refractive Index 2.2532.253
 
Descriptive Properties
CAS Number7785-23-1
Crystal StructureCubicSphalerite Structure - Space Group F(-4)3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1070 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1074 Steel, hot rolled, (discontinued)
AISI 1080 Steel, annealed at 790°C (1450°F), furnace cooled 11°C (20°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
AISI 1080 Steel, annealed at 790°C (1450°F)
AISI 1074 Steel, cold rolled strip (discontinued)

DSEN42 / 3054

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.