MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi PEI ULTEM™ 1010 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: PEI ULTEM™ 1010 is an ultra-performance with exceptional dimensional stability, inherent flame retardancy and good chemical resistance. PEIULTEM™ 1010 is a material from SABIC. This material is an amorphous, amber to transparent thermoplastics with a glass transition temperature (Tg) of 217? and performs in continuous use up to 170?. PEIULTEM™ 1010 offers superior tensile strength and excellent chemical and thermal resistance for an FDM thermoplastic.

Features:

  • Low smoke evolution
  • High thermal properties 217? (Tg)
  • Dimensional stability
  • Flame retardant
  • Outstanding strength and amorphous thermoplastic
Colors: PEI ULTEM™1010 is available in the color natural

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccISO 1183
Filament Diameter 1750 µm1750 µmTolerance: 50 µm, =95% Roundness
 2850 µm2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 340 °C
11 g/10 min
@Load 11.0 lb,
Temperature 644 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 540 MPa78300 psiISO 527
Tensile Strength, Yield 105 MPa15200 psiISO 527
Elongation at Break 60 %60 %ISO 527
Elongation at Yield 6.0 %6.0 %ISO 527
Tensile Modulus 3.20 GPa464 ksi(E); ISO 527
Flexural Strength 160 MPa23200 psiISO 178
Flexural Modulus 3.20 GPa464 ksiISO 178
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FISO 75-2
Vicat Softening Point 211 °C412 °FISO 306 B50
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 355 - 385 °C671 - 725 °FPrinting Temperature
Drying Temperature 110 °C230 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
Bed Temp=120°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9832 / 301057

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.