MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hapco Hapflex 660-3 Semi-rigid urethane elastomers
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: The Hapflex 600 series products are known for their superior impact and abrasion resistance. Products in this series possess flame retardant properties and perform excellently in high or low temperatures. When post-cured, these products are virtually unbreakable. Living hinges, protective coverings, forming dies, patterns and core boxes are just a few examples of 600 Series applications.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D-4669
Viscosity 1560 cP1560 cPASTM D-4878
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D-2240
Tensile Strength 19.3 MPa2800 psiASTM D-638
Elongation at Break 225 %225 %ASTM D-638
Modulus of Elasticity 0.138 GPa20.0 ksiASTM D-638
Flexural Strength 11.4 MPa1660 psiASTM D-790
Flexural Modulus 0.170 GPa24.6 ksiASTM D-790
Izod Impact, Notched 1.17 J/cm2.20 ft-lb/inASTM D-256
Izod Impact, Unnotched NBNBASTM D-256
Tear Strength 73.6 kN/m420 pliASTM 624 Die C
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °FASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 20.0 - 35.0 min
@Thickness 3.17 mm
0.333 - 0.583 hour
@Thickness 0.125 in
Demold
Gel Time 3.00 min
@Load 0.100 kg
3.00 min
@Load 0.221 lb
ASTM D-2971
 
Descriptive Properties
Color (cured)Black
Mix Ratio100:55Volume
 100:60Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAPCO100 / 317159

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.