MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Amodel® AS-1933 HS PPA, 33% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 33% glass fiber, for thick-wall parts (>3mm), glycol resistant, heat stabilized

Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material exceeds the performance required by the automotive industry for polymeric materials exposed to antifreeze at 226°F (108°C), even when tested at 275°F (135°C).

Potential applications include a variety of automotive components such as thermostat housings, heater core endcaps, heater hose connectors, and water inlets, outlets and valves.

- Black: AS-1933 HS BK 324

Applications: Automotive Applications; Automotive Under the Hood; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts

Features: Antifreeze Resistant; Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Glycol Resistance; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength

Injection notes: Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³Method A; ISO 1183
Water Absorption 0.21 %
@Time 86400 sec
0.21 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.8 MPa11000 psiASTM D638
 212 MPa30700 psiISO 527-2
 221 MPa32100 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
 2.5 %2.5 %ISO 527-2
Tensile Modulus 7.58 GPa1100 ksiASTM D638
 11.7 GPa1700 ksiASTM D638
 12.6 GPa1830 ksiISO 527-2
Flexural Strength 309 MPa44800 psiISO 178
Flexural Yield Strength 313 MPa45400 psiASTM D790
Flexural Modulus 10.6 GPa1540 ksiISO 178
 10.8 GPa1570 ksiASTM D790
Izod Impact, Notched 0.530 - 0.910 J/cm0.993 - 1.70 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 9.50 kJ/m²4.52 ft-lb/in²Type 1, Notch A; ISO 180
Charpy Impact Unnotched 7.60 J/cm²36.2 ft-lb/in²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 312 °C594 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 277 °C531 °FUnannealed; ASTM D648
 278 °C532 °FUnannealed, Flatwise; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Feed Temperature 79.0 °C174 °FInjection Hopper
Rear Barrel Temperature 304 - 318 °C579 - 604 °F
Front Barrel Temperature 316 - 329 °C601 - 624 °F
Melt Temperature 321 - 343 °C610 - 649 °FInjection
Mold Temperature 135 °C275 °F
Drying Temperature 121 °C
@Time 14400 sec
250 °F
@Time 4.00 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4086 / 279886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.