MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Free Form™ Habitat® Fire Safe Epoxy Putty
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: Free Form™ Habitat™ Fire Safe™ epoxy putty is a high density epoxy sculpting putty that is flame rated (E84, Class A). Habitat™ Fire Safe™ is solvent-free and contains no VOC’s. Working time is 90 minutes and cure time is 16 hours at room temperature (73° F/23° C). Epoxy cures to a very hard, flame and heat resistant material that is easily painted. Habitat™ Fire Safe™ does not contain any carcinogens (cancer causing agents). Free Form™ Habitat™ Fire Safe™ is suitable for interior and exterior theming applications and general sculpting. It is also certified ‘aquarium safe’ and is used by aquariums and zoos to make hyper-realistic trees, vines, rocks, coral and other display elements. Use with Habitat™ Folding Powder – fold powder into epoxy putty to thicken and reduce sag when applied to a vertical surface. Folding Powder also reduces stickiness and makes the epoxy more handle-able. Once putty is applied, it can be stamped with a silicone rubber stamp to create repeating patterns with intricate detail over a large surface area. Surface can be smoothed with alcohol or water. New Habitat™ Fire Safe™ will bond to cured Habitat™ Fire Safe™ without delamination. Habitat™ Fire Safe™ will not melt foam, and can be used as an EPS foam coating. Free Form™ Habitat™ Fire Safe™ is also an excellent repair cement and bonds permanently to itself, PVC, Plexiglas™ (acrylic), wood, many metals, plastics and foams.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D-1475
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D-2240
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 77.0 °C171 °FHeat Deflection Temperature; ASTM D-648
 100 °C212 °FDeflection Temp. Post cured per heat post curing schedule; ASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min16.0 hour
Pot Life 90.0 min90.0 minASTM D-2471
 
Descriptive Properties
ColorNeutral
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Mixed ViscosityDough
Specific Volume17.3[in3/lb], ASTM D1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN214 / 296915

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.