Temper: As Centrifugal Cast Casting Characteristics: High – Shrinkage in Solidification, Drossing; Medium – Fluidity; Low – Casting Yield, Effect of Section Size, Gassing Fabrication Properties: Good Suitability – Oxyacetylene Welding, Coated Metal Arc Welding; Fair Suitability – Gas Shielded Arc Welding; Poor Suitability – Soldering, Brazing Typical uses: Brackets; Structural Parts; Screw Down Nuts; Bushings; Cams; Frames; Gears; High Strength Machine Parts; Hooks; Marine Racing Propellers; Pressing Dies for Wood Pulp; Shafts; Valve Stems; Wear Rings for Pressing Dies for Wood Pulp Industry; Worm Gears; Boat Parts; Clamps; Marine Castings; Rudders; Gun Mounts Applicable Specifications: As Centrifugal Cast - Castings SAE J462, Castings ASTM B271/B271M, Castings SAE J461; As Continuous Cast – Castings SAE J461, Castings SAE J462, Castings – ASTM B505/B505M; As Sand Cast – Castings ASTM B584, ASTM B763/B763M, Castings SAE J462, Castings SAE J461; Ingot - ASTM B30, FEDERAL QQ-C-523; Precision Cast – Castings MILITARY MIL-C-11866 |