MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Staybelite™ Ester 5-E Resin
Categories: Polymer

Material Notes: Product Description: Staybelite™ Ester 5-E Resin is a pale, medium-hard, thermoplastic synthetic resin that has excellent resistance to oxidation, discoloration, and other properties affected by ageing. It is the glycerol ester of partially hydrogenated rosin specially processed to yield a low-odor, low-acidnumber product. These and other outstanding properties make it particularly useful as a modifier of masticatory ingredients used in chewing gum bases.

Application/Uses:

  • Chewing Gum
  • Hot Melt Adhesives
  • Solventborne Adhesives
  • Wax Modification
Key Attributes:
  • Excellent chewing gum base
  • Excellent resistance to oxidation
  • Light color
  • Low odor
  • Medium softening point
  • Thermoplastic hydrogenated resin
  • Wide solubility and compatibility range

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/cc
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 7.0[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Softening Point 86.0 °CHercules drop method
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 6.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5589 / 222783

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.