MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Bergadur™ PB400 G15 H UF UV Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/ccISO 1183
Filler Content 15 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0040 - 0.0090 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 78.5 MPa
@Temperature 23.0 °C
ISO 527-2/5
Flexural Strength 156 MPaISO 178
Flexural Modulus 6600 MPaISO 178
Charpy Impact, Notched 6.40 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+14 ohmASTM D257
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 198 °CUnannealed; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.800 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 260 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 110 - 120 °C
Dry Time 4.00 - 6.00 hour
 
Descriptive Properties
AdditiveUV Stabilizer
AppearanceNatural Color
FeaturesFlame Retardant
 Halogen Free
FormsPellets
Generic MaterialPBT
Generic NamePolybutylene Terephthalate (PBT)
Regional AvailabilityAsia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Crastin® SK643FR BK851 PBT-GF20FR(17)
DuPont Mobility and Materials Minlon® 22C BK086 PA66-(MD+GF)38
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Evonik Vestamid® L1600 nf (dry properties) Nylon 12
Avient Bergadur™ PB40 G30 UF UV Polybutylene Terephthalate (PBT)

PH0POL1122 / 145691

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.