Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.23 g/cc | 1.23 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 90 | 90 |
| 70 @Treatment Temp. 23.0 °C, Time 252000 sec | 70 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 74 @Treatment Temp. 23.0 °C, Time 252000 sec | 74 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 85 @Treatment Temp. 100 °C, Time 252000 sec | 85 @Treatment Temp. 212 °F, Time 70.0 hour |
| 89 @Treatment Temp. 23.0 °C, Time 252000 sec | 89 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 89 @Treatment Temp. 100 °C, Time 252000 sec | 89 @Treatment Temp. 212 °F, Time 70.0 hour |
| 90 @Treatment Temp. 150 °C, Time 252000 sec | 90 @Treatment Temp. 302 °F, Time 70.0 hour |
| 90 @Treatment Temp. 100 °C, Time 252000 sec | 90 @Treatment Temp. 212 °F, Time 70.0 hour |
| 90 @Treatment Temp. 125 °C, Time 252000 sec | 90 @Treatment Temp. 257 °F, Time 70.0 hour |
| 94 @Treatment Temp. 125 °C, Time 252000 sec | 94 @Treatment Temp. 257 °F, Time 70.0 hour |
| 94 @Treatment Temp. 100 °C, Time 252000 sec | 94 @Treatment Temp. 212 °F, Time 70.0 hour |
| 96 @Treatment Temp. 125 °C, Time 252000 sec | 96 @Treatment Temp. 257 °F, Time 70.0 hour |
| 96 @Treatment Temp. 150 °C, Time 252000 sec | 96 @Treatment Temp. 302 °F, Time 70.0 hour |
Tensile Strength | 23.08 MPa | 3348 psi |
| 12.211 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1771.1 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 16.181 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 2346.9 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 21.698 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 3147.1 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 22.183 MPa @Treatment Temp. 150 °C, Time 252000 sec | 3217.4 psi @Treatment Temp. 302 °F, Time 70.0 hour |
| 25.346 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3676.1 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 27.054 MPa @Treatment Temp. 125 °C, Time 252000 sec | 3923.9 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 27.885 MPa @Treatment Temp. 100 °C, Time 252000 sec | 4044.4 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 28.92 MPa @Treatment Temp. 100 °C, Time 252000 sec | 4195 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 28.970 MPa @Treatment Temp. 125 °C, Time 252000 sec | 4201.7 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 28.993 MPa @Treatment Temp. 150 °C, Time 252000 sec | 4205.1 psi @Treatment Temp. 302 °F, Time 70.0 hour |
| 29.92 MPa @Treatment Temp. 125 °C, Time 252000 sec | 4339 psi @Treatment Temp. 257 °F, Time 70.0 hour |
Elongation, Ultimate | 220 % | 220 % |
| 100 % @Treatment Temp. 125 °C, Time 252000 sec | 100 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 100 % @Treatment Temp. 150 °C, Time 252000 sec | 100 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 100 % @Treatment Temp. 150 °C, Time 252000 sec | 100 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 125 °C, Time 252000 sec | 130 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 23.0 °C, Time 252000 sec | 130 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 125 °C, Time 252000 sec | 130 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 100 °C, Time 252000 sec | 130 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 139.9 % @Treatment Temp. 100 °C, Time 252000 sec | 139.9 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 159.9 % @Treatment Temp. 100 °C, Time 252000 sec | 159.9 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 190.1 % @Treatment Temp. 23.0 °C, Time 252000 sec | 190.1 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 199.98 % @Treatment Temp. 23.0 °C, Time 252000 sec | 199.98 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
100% Modulus | 11.39 MPa | 1652 psi |
Tear Strength | 45.6 kN/m | 260 pli |
| 62.9 kN/m | 359 pli |
Compression Set | 18.9 % @Treatment Temp. 100 °C, Time 79200 sec | 18.9 % @Treatment Temp. 212 °F, Time 22.0 hour |
| 22 % @Treatment Temp. 125 °C, Time 79200 sec | 22 % @Treatment Temp. 257 °F, Time 22.0 hour |
| 24.7 % @Treatment Temp. 100 °C, Time 79200 sec | 24.7 % @Treatment Temp. 212 °F, Time 22.0 hour |
| 35.7 % @Treatment Temp. 125 °C, Time 79200 sec | 35.7 % @Treatment Temp. 257 °F, Time 22.0 hour |
| 37.1 % @Treatment Temp. 100 °C, Time 252000 sec | 37.1 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 49.9 % @Treatment Temp. 100 °C, Time 252000 sec | 49.9 % @Treatment Temp. 212 °F, Time 70.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -33.9 °C | -29.0 °F |
Shrinkage | -4.60 % @Treatment Temp. 150 °C, Time 252000 sec | -4.60 % @Treatment Temp. 302 °F, Time 70.0 hour |
| -4.20 % @Treatment Temp. 125 °C, Time 252000 sec | -4.20 % @Treatment Temp. 257 °F, Time 70.0 hour |
| -3.20 % @Treatment Temp. 100 °C, Time 252000 sec | -3.20 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 1.4 % @Treatment Temp. 23.0 °C, Time 252000 sec | 1.4 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 6.9 % @Treatment Temp. 100 °C, Time 252000 sec | 6.9 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 10.3 % @Treatment Temp. 125 °C, Time 252000 sec | 10.3 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 11.7 % @Treatment Temp. 150 °C, Time 252000 sec | 11.7 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 12.2 % @Treatment Temp. 100 °C, Time 252000 sec | 12.2 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 29.1 % @Treatment Temp. 23.0 °C, Time 252000 sec | 29.1 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 47.8 % @Treatment Temp. 23.0 °C, Time 252000 sec | 47.8 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |