MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Universal Wire Works EZ33A (AMS 4396) Magnesium Alloy Filler Metal
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Magnesium alloy EZ33A is used primarily for inert gas arc welding of base metals of similar composition.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Cerium, Ce 3.5 %3.5 %
Copper, Cu 0.10 %0.10 %
Magnesium, Mg >= 92.39 %>= 92.39 %As Remainder
Nickel, Ni <= 0.010 %<= 0.010 %
Other <= 0.30 %<= 0.30 %
Zinc, Zn 2.8 %2.8 %
Zirconium, Zr 0.90 %0.90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2024-O
COI Ceramics Nextelâ„¢ A-N720 Oxide Ceramic Matrix Composite, Alumina
Aluminum A356.0-T6, Sand Cast
Magnesium AZ91A-F, Die Cast
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3

NUWW204 / 19688

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.