Description: - High permeability, magnetic absorber.
- Low magnetic loss (µ”) below 100 MHz makesWX-B0301 ideal for antenna miniaturization.
- Standard sheet size: 12” x 12” (30.48 cm x 30.48 cm); Other sheet sizes available upon request.
- Standard sheet thickness: 0.020” (0.508 mm)
- This product can be provided with PSA, and can be water-jet or die cut into custom shapes.