MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Teijin Films Mylar® RB5 Polyester Packaging Film, 100 Gauge  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

Mylar® RB5 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer and a polyvinylidene chloride (PVDC) barrier layer "buried" between the OPET base and the EVA heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods.

Mylar® RB5 is designed to seal to a broad range of container substrates including amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, polyvinylchloride (PVC), polyethylene (HDPE), polypropylene (PP), and polystyrene (HIPS). Mylar® RB5 has the same type and thickness of heat seal layer as Mylar® RL32. The heat seal strengths of Mylar® RB5 are intermediate between Mylar® RL31 and Mylar® RL33. Like Mylar® RL32, Mylar® RB5 has a lower seal initiation temperature than lidding films with an amorphous polyester heat seal layer (e.g., Mylar® OL, OL2). This allows good seals to be made at higher line speeds (or using lower sealing temperatures).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³Calculated from nominal thickness and yield
Moisture Vapor Transmission 0.610 cc-mm/m²-24hr-atm1.55 cc-mil/100 in²-24hr-atmProc. E; ASTM E96
Oxygen Transmission 2.36 cc-mm/m²-24hr-atm5.99 cc-mil/100 in²-24hr-atmTested per ASTM D3985 at 22°C
Thickness 25.4 microns1.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 110 %110 %ASTM D882
Film Elongation at Break, TD 80 %80 %ASTM D882
Secant Modulus 3.79 GPa550 ksiStiffness Modulus; ASTM D882
Tear Strength Test 1.11.1lb Graves; ASTM D1004
Film Tensile Strength at Break, MD 172 MPa24900 psiASTM D882
Film Tensile Strength at Break, TD 241 MPa35000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) HIPS 7240 High Impact Polystyrene
INEOS Styrolution PS 495N HIPS
INEOS Styrolution PS 454N HIPS
I. Stern HIPS 8 High Impact Polystyrene Injection Grade
E-Polymers TEKAPPO® JF101 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO

PDU7J7 / 33287

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.