MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASINT 3012 Polyimide, Ochre Brown (PI)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.

Main features: High thermal stability, very creep resistant, good radiation-resistance, low outgassing, good chemical resistance, flame retardant according to UL94 V-0, easily machined, sensitive to hydrolysis in higher thermal range, very good electrical insulation

Applications: Mechanical engineering, vacuum technology, electrical engineering, cryogenics, precision engineering, aircraft and aerospace industries, glass technology, conveyor technology

Preferred Fields: Valve seats, insulators, switch parts, wear sensor for brakes, carriage

Information Provided by Ensinger Sintimid

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³DIN 53 479
Water Absorption  0.80 %
@Temperature 23.0 °C
0.80 %
@Temperature 73.4 °F
24 hours in water; EN ISO 62
 2.58 %
@Temperature 80.0 °C
2.58 %
@Temperature 176 °F
24 hours in water; EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80
@Temperature 23.0 °C
80
@Temperature 73.4 °F
DIN 53 505
Tensile Strength 57.4 MPa
@Temperature 23.0 °C
8330 psi
@Temperature 73.4 °F
EN ISO 527
Elongation at Break 6.0 %
@Temperature 23.0 °C
6.0 %
@Temperature 73.4 °F
EN ISO 527
Tensile Modulus 2.284 GPa
@Temperature 23.0 °C
331.3 ksi
@Temperature 73.4 °F
EN ISO 527
Flexural Strength 81.0 MPa
@Temperature 23.0 °C
11700 psi
@Temperature 73.4 °F
EN ISO 178
Flexural Modulus 2.215 GPa
@Temperature 23.0 °C
321.3 ksi
@Temperature 73.4 °F
EN ISO 178
Flexural Strain at Yield 7.9 %
@Temperature 23.0 °C
7.9 %
@Temperature 73.4 °F
EN ISO 178
Compressive Yield Strength 82.0 MPa
@Strain 10 %,
Temperature 23.0 °C
11900 psi
@Strain 10 %,
Temperature 73.4 °F
EN ISO 604
Compressive Strength 389 MPa
@Temperature 23.0 °C
56400 psi
@Temperature 73.4 °F
EN ISO 604
Compressive Modulus 1.135 GPa
@Temperature 23.0 °C
164.6 ksi
@Temperature 73.4 °F
EN ISO 604
Charpy Impact Unnotched 3.11 J/cm²
@Temperature 23.0 °C
14.8 ft-lb/in²
@Temperature 73.4 °F
EN ISO 179
Charpy Impact, Notched 0.560 J/cm²
@Temperature 23.0 °C
2.66 ft-lb/in²
@Temperature 73.4 °F
EN ISO 179
Compression Set 66.3 %
@Temperature 23.0 °C
66.3 %
@Temperature 73.4 °F
Compression at Break; EN ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear  54.0 µm/m-°C
@Temperature 50.0 - 200 °C
30.0 µin/in-°F
@Temperature 122 - 392 °F
DIN 53 752
 71.0 µm/m-°C
@Temperature 200 - 300 °C
39.4 µin/in-°F
@Temperature 392 - 572 °F
DIN 53 752

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hippe PI
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
Ensinger TECASINT™ 2021 Polyimide, Brown (PI)
Ensinger XP-131 Compression Molded Unfilled PI
Ensinger TECASINT 1041 Polyimide, 30% MoS2 Filled (PI)

PENSIN075 / 121078

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.