MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Park Aerospace Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applications that require optimum signal integrity and precise impedance control, while maintaining high reliability through CAF and thermal resistance.

Key Features and Benefits:

  • Lead-Free Assembly Compatible
  • Tg >210ºC, outstanding thermal, electrical and signal loss properties
  • CAF Resistant
  • Signal Integrity and Buried Capacitance™ Options
  • High-Tg FR-4 processing
  • Available in a variety of constructions

Applications/Qualifications:

  • Fine-Line Multilayers
  • Backplanes
  • Surface-Mount Multilayers
  • BGA Multilayers
  • MCM-Ls
  • CSP Attachment
  • Wireless Communications Infrastructure
  • High Speed Services
  • High Speed Storage Networks
  • Internet Switching / Routing Systems

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.79 g/cc0.0647 lb/in³50% Resin Content; Internal Method
Water Absorption 0.10 %0.10 %IPC-TM-650.2.6.2.1
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 15.9 GPa2300 ksiY; ASTM D3039
 16.5 GPa2400 ksiX; ASTM D3039
Poissons Ratio 0.170.17Y; ASTM D3039
 0.180.18X; ASTM D3039
Peel Strength 1.31 kN/m7.50 pliafter solder float; IPC-TM-650.2.4.8
 1.42 kN/m8.10 pliat elevated temperature; IPC-TM-650.2.4.8.2a
 1.58 kN/m9.00 pliafter exposure to process solutions; IPC-TM-650.2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmC - 96/35/90; IPC-TM-650.2.5.17.1
 1.00e+14 ohm-cm1.00e+14 ohm-cmE - 24/125; IPC-TM-650.2.5.17.1
Surface Resistance 1.00e+13 ohm1.00e+13 ohmC - 96/35/90; IPC-TM-650.2.5.17.1
 1.00e+13 ohm1.00e+13 ohmE - 24/125; IPC-TM-650.2.5.17.1
Dielectric Constant  3.2
@Frequency 2.50e+9 Hz
3.2
@Frequency 2.50e+9 Hz
Split Post Cavity
 3.2
@Frequency 1e+10 Hz
3.2
@Frequency 1e+10 Hz
Stripline; IPC-TM-650.2.5.5.5
 3.3
@Frequency 1e+10 Hz
3.3
@Frequency 1e+10 Hz
Split Post Cavity
 3.4
@Frequency 1e+9 Hz
3.4
@Frequency 1e+9 Hz
RF Impedance; IPC-TM-650.2.5.5.9
Dielectric Strength 39.4 kV/mm1000 kV/inIPC-TM-650.2.5.6.2
Dielectric Breakdown >= 50000 V>= 50000 VIPC-TM-650.2.5.6
Dissipation Factor  0.0070
@Frequency 1e+10 Hz
0.0070
@Frequency 1e+10 Hz
Split Post Cavity
 0.0080
@Frequency 2.50e+9 Hz
0.0080
@Frequency 2.50e+9 Hz
Split Post Cavity
 0.0080
@Frequency 1e+10 Hz
0.0080
@Frequency 1e+10 Hz
Stripline; IPC-TM-650.2.5.5.5
Arc Resistance 123 sec123 secIPC-TM-650.2.5.1
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.00 - 13.0 µm/m-°C
@Temperature -40.0 - 125 °C
5.00 - 7.23 µin/in-°F
@Temperature -40.0 - 257 °F
X/Y; IPC-TM-650.2.4.41
 70.06 µm/m-°C
@Temperature 50.0 - 210 °C
38.92 µin/in-°F
@Temperature 122 - 410 °F
Z-Axis Alpha 1; IPC-TM-650.2.4.41
 280.22 µm/m-°C
@Temperature 210 - 260 °C
155.68 µin/in-°F
@Temperature 410 - 500 °F
Z-Axis Alpha 2; IPC-TM-650.2.4.41
Specific Heat Capacity 1.30 J/g-°C0.310 BTU/lb-°FASTM E1461
Thermal Conductivity 0.294 W/m-K2.04 BTU-in/hr-ft²-°FASTM E1461
Glass Transition Temp, Tg 200 °C392 °FTMA; IPC-TM-650.2.4.24c
 210 °C410 °FDSC; IPC-TM-650.2.4.25c
 240 °C464 °FDMA (Tan d Peak); IPC-TM-650.2.4.24.3
Decomposition Temperature 350 °C662 °F5% weight loss; TGA; IPC-TM-650.2.4.24.6
Flammability, UL94 V-0V-0
 
Descriptive Properties
Methylene Chloride Resistance (% Weight Change)0.7IPC-TM-650.2.3.4.3
Pressure CookerPass60 min then solder dip @288ºC until failure (max 10 min.); IPC-TM-650.2.6.16 (modified)
T260 (minutes)>30IPC-TM-650.2.4.24.1
T288 (minutes)>10IPC-TM-650.2.4.24.1
Z Axis Expansion (%)3.550ºC to 260ºC; IPC-TM-650.2.4.41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Park Aerospace Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg
Park Aerospace Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg
Park Aerospace Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg
Park Aerospace Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg
Park Aerospace Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg

PPARK107 / 89379

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.