MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaofil HT Pumpable
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kaofil Pumpables are a mixture of Kaowool ceramic fibers and fillers dispersed in a high-temperature binder. This mix produces a stable high-temperature insulation which can be placed by forced pumping such as through a Kaowool Diaphragm Pump or a piston extrusion pump.

Kaofil Pumpables can be used in hot or cold repairs. These pumpables will air dry over time. However, at unit operating temperatures, the drying is rapid while still allowing time for the pumpable, under force, to seek out voids. Kaofil Pumpables offer good insulating properties, good strength and vibration resistance.

Features:

  • Hot spot repair
  • One-component pumpable
  • Ready to use
  • Good damming ability
  • Highly insulating
  • Applications:

  • Hot or cold repair to refractory backup insulation
  • Hot or cold repair of boiler insulation, sidewalls, and penthouses
  • Brick kiln crown and walls
  • Coke oven jambs and seals
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density >= 0.625 g/cc>= 0.0226 lb/in³dried
    Solids Content 46 %46 %
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.00138 GPa0.200 ksidried
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0865 W/m-K
    @Temperature 149 °C
    0.600 BTU-in/hr-ft²-°F
    @Temperature 300 °F
    ASTM C417
     0.115 W/m-K
    @Temperature 371 °C
    0.800 BTU-in/hr-ft²-°F
    @Temperature 700 °F
    ASTM C417
     0.159 W/m-K
    @Temperature 593 °C
    1.10 BTU-in/hr-ft²-°F
    @Temperature 1100 °F
    ASTM C417
    Melting Point 1760 °C3200 °F
    Maximum Service Temperature, Air 1320 °C2400 °F
    Shrinkage  -2.50 %
    @Temperature 1260 °C,
    Time 18000 sec
    -2.50 %
    @Temperature 2300 °F,
    Time 5.00 hour
     -1.00 %
    @Temperature 1090 °C,
    Time 18000 sec
    -1.00 %
    @Temperature 2000 °F,
    Time 5.00 hour
     
    Processing PropertiesMetricEnglishComments
    Shelf Life 6.00 Month6.00 Month
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 40 %40 %
    SiO2 60 %60 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM268 / 2588

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.