MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sandvik Cuprothal SX Thermocouple
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: CUPROTHAL SX is the negative leg of compensating cables for thermocouple type S/R.CUPROTHAL must be matched with electrolytic copper (ASTM B3) to meet the reference standard.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 330 MPa
@Thickness 0.320 mm
47900 psi
@Thickness 0.0126 in
Elongation at Break 30 %
@Thickness 0.320 mm
30 %
@Thickness 0.0126 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000120 ohm-cm0.0000120 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
8.89 µin/in-°F
@Temperature 68.0 - 212 °F
Melting Point 1080 °C1980 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 95 %95 %
Manganese, Mn 2.0 %2.0 %
Nickel, Ni 3.0 %3.0 %
 
Descriptive Properties
emf, mV, Reference junction 0°C0.646; at 100°C
 1.441; at 200°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV108 / 19002

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.