MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.

Key applications for Akulon:

  • Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectors
  • Consumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, Transportation
  • E&E: Low voltage switch gear/power distribution, Lighting, Power connectors
  • Film: Specialty and barrier films

Information provided by DSM.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Water Absorption 6.2 %6.2 %Sim. to ISO 62
Moisture Absorption at Equilibrium 1.8 %1.8 %Humidity Absorption; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4
Melt Flow 27.6 g/10 min
@Load 2.16 kg,
Temperature 250 °C
27.6 g/10 min
@Load 4.76 lb,
Temperature 482 °F
Calculated from Volume Flow Rate of 20 cm3/10min.; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527-1/-2
Elongation at Break 3.0 %3.0 %ISO 527-1/-2
Tensile Modulus 6.20 GPa899 ksiISO 527-1/-2
Charpy Impact Unnotched 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 >= 600 V>= 600 VPLC 0; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 20.0 °C
27.8 µin/in-°F
@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 20.0 °C
27.8 µin/in-°F
@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 220 °C428 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FISO 75-1/-2
UL RTI, Electrical  65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
UL746B
 65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL746B
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL746B
 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
UL746B
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
UL746B
 65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL746B
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
IEC 60695-11-10
 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
IEC 60695-11-10
Glow Wire Ignition Temperature  700 °C
@Thickness 0.750 mm
1290 °F
@Thickness 0.0295 in
IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
1340 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Descriptive Properties
Flame RetardantYes
Flame Retarding AgentYes
Heat Stabilized or Stable to HeatYes
Injection MoldingYes
Release AgentYes
RSV Formic Acid2.25 g/100mlISO 307
With FillersYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSMEU062 / 31152

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.