MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
IRPC Polimaxx Pentfoam 255E Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: General: Pentfoam 255E is a self extinguishing grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast expansion rate and short pressure release times in block molding.

Applications: Pentfoam 255E is particularly well suited for hte manufacture of self extinguishing eps insulation boards, block molded or produced in continuous molding machines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0130 - 0.0140 g/cc
 0.0140 - 0.0250 g/ccmolding density range
Bead Size 1.00 - 1.60 mm
Maximum Moisture Content 0.20
 
Chemical PropertiesOriginal ValueComments
Blowing Agent Content >= 5.9 %
 
Mechanical PropertiesOriginal ValueComments
K Factor (Wear Factor) 54.5 - 58.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Extir® D 3000 AE Expandable Polystyrene - Flame Retardant
BASF Styropor® BFL 222 EPS
BASF Peripor® 200 Expandable Polystyrene
BASF Neopor® 2400 Expandable Polystyrene
Bamberger Polymers Bapolan® 6045 Polystyrene, Injection Grade

PIRPC018 / 83995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.