MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Sultex® F
Categories: Fluid; Lubricant

Material Notes: Texaco Sultex delivers value through:
  • Heavy duty performance — Texaco Sultex oils are designed for tough machining operations on difficult to machine metals and alloys.
  • Low tool wear — Special compounding provides excellent lubricity and antiweld properties.
  • Good surface finishes — Chip welding is highly reduced. Surface of finished parts come out extremely fine, producing high quality work.

Texaco Sultex oils are dark, active sulfur, heavy duty cutting oils. They contain highly effective EP and lubricity additives that provide maximum cutting performance. They should not be used to machine copper or its alloys.

Texaco Sultex cutting oils:

  • provide excellent cooling and lubrication in a wide range of machining operations
  • prevent welding of chip and tool
  • protect the finished work surfaces, tools and machine against rust and corrosion
  • provide long tool life and excellent surface finish
  • flush chips away from the work area
  • reduce oil mist in high-speed machine tools

Texaco Sultex cutting oils are formulated with paraffinic base stocks with a naturally high viscosity index. These cutting oils have high flash points, minimizing the potential for fire

Texaco Sultex oils possess the highest level of EP and antiweld properties.

Texaco Sultex D and F are recommended for difficult machining operations, such as tapping, threading, broaching, gear cutting and form grinding. They are suited for machining of ferrous alloys with machinability ratings below 70%

Texaco Sultex F contains a higher level of fatty oil to provide good surface finishes in severe machining operations. Texaco Sultex F may also be used to fortify lighter-duty cutting oils for more severe operations.

Texaco Sultex oils are also suitable for drawing and stamping operations on difficult to machine metals and alloys.

Texaco Sultex oils contain active sulfur that is staining to yellow metals. Texaco Sultex oils should not be used to machine copper and its alloys.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221585; MSDS Number: 8904

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 27.1 °27.1 °
Saybolt Viscosity at 100°F 240 SUS240 SUS
Saybolt Viscosity at 210°F 51 SUS51 SUS
Kinematic Viscosity at 40°C (104°F) 46.7 cSt46.7 cSt
Kinematic Viscosity at 100°C (212°F) 7.3 cSt7.3 cSt
ASTM Color 8.08.0D
 
Descriptive Properties
ChlorineNone
Fatty OilPresent
PhosphorusPresent
SulfurPresent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WTEXA295 / 77174

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.