ZEON HyTemp® 4454 AR Polyacrylate Elastomer
Categories:
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
Material Notes:
HyTemp 4454 is a ground form of HyTemp 4054, which contains one or more acrylic esters with a small percentage of a carboxy/chlorine cure site.
Particulate version of HyTemp 4054.
Key Words:
ACM
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.10
g/cc
1.10
g/cc
Mooney Viscosity
22 - 34
@Temperature 100 °C
22 - 34
@Temperature 212 °F
(1+4); Zeon Test #404
Ash
<= 0.60 %
<= 0.60 %
Zeon Test #873
Thermal Properties
Metric
English
Comments
Minimum Service Temperature, Air
-41.0
°C
-41.8
°F
Gehman T100
Glass Transition Temp, Tg
-40.6
-
-31.7
°C
-41.1
-
-25.1
°F
Zeon Test #1273
Descriptive Properties
% Volume Swell
63
Curesite
Dual
Gel-Mek (%), max
20
Heat Loss (%) Max
0.5
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
AISI 1018 Steel, hot rolled, quenched, and tempered
AISI 1018 Steel, cold drawn
PZEONC30 / 73089
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.