MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes: Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These properties make the Lastanes very suitable for wheels, gears, couplings, parts of textile machinery, shoes, and others. Reinforced Lastanes are used when good rigidity and high dimensional stability are required.

Specific Notes for this Material: 40% glass fiber; very low molding shrinkage; good dimensional stability; good noise inertness; good rigidity; good impact resistance even at low temperatures.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ISO 1183
Water Absorption 0.30 %0.30 %at 23°C; ISO 62
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inLATI
Linear Mold Shrinkage, Transverse 0.0020 cm/cm0.0020 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 75.0 MPa10900 psiISO 527
Flexural Modulus 2.30 GPa334 ksiASTM D790
Izod Impact, Notched 6.00 J/cm11.2 ft-lb/inASTM D256
 2.00 J/cm
@Temperature -40.0 °C
3.75 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 4.00 J/cm
@Temperature -20.0 °C
7.49 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched >= 30.0 J/cm²>= 143 ft-lb/in²DIN 53453
 6.50 J/cm²
@Temperature -40.0 °C
30.9 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 8.00 J/cm²
@Temperature -20.0 °C
38.1 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 115 °C239 °F50°C/h 50N; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 220 °C392 - 428 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 80.0 - 100 °C176 - 212 °FNecessary, temperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourNecessary, drying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Injection Speedmedium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced
LATI Lastane 50 PUR
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Arkema Evatane® 1003 VL 4C Ethylene Vinyl Acetate
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate

PLATI142 / 50140

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.