MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Excelite Plastic Fluorescent Polycarbonate sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: The Fluorescent edge effect is one of the most popular choices of designers and fabricators who want their ideas to catch the eye. TOP Fluorescent combines a delicate transparent tinted sheet with a striking fluorescent edge which adds a contemporary touch to point of sale designs and displays.
  • Subtle transparent tints
  • Striking fluorescent edge
  • Exciting contemporary colors
  • Superb cutting and fabrication
  • Excellent aesthetics
  • Ideal for in store displays, POP, furnishings and shelving
In retail display every inch of floor space is precious and POP displays need something extra to attract attention. Fluorescent offers designers a range of exciting colors with a vivid fluorescent edge effect. that will make any design stand out from the crowd.Applications:
  • POP
  • Display units
  • Interior signs and signage
  • Interior fittings and furnishings

Information provided by Excelite Plastic Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccGB/T 1033
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
GB/T 1033
Thickness 1500 - 12000 microns59.1 - 472 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.3 MPa8750 psiGB/T 1040
Elongation at Break >= 90 %>= 90 %GB/T 1040
 108 %108 %Tensile; GB/T 1040
Elongation at Yield 6.0 %6.0 %GB/T 1040
Modulus of Elasticity 0.240 GPa34.8 ksiGB/T 9341
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°FGB/T 1034
 
Descriptive Properties
ColorRed, Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Plexiglas® 45 Resist® Extruded Acrylic
Röhm Acrylite® SG Acrylic Sheet, Sign Grade
LNP Lexan® BFL3501 Polycarbonate
Covestro Makrolon® ET 3137 Polycarbonate

PEXLT004 / 198714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.