MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Bormed™ LE6600-PH LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Bormed" LE6600-PH is a resin intended for evaluation for use in Healthcare applications. Bormed" LE6600-PH is an additive free low density polyethylene which is used to produce soft and flexible packaging for pharmaceutical products. The material can be converted via blow molding, including blow-fill-seal technology, or IBM into small bottles or ampoules. It can also be used in injection molding and blown film process. It is produced using tubular technology. The Bormed" concept is based on the three core principles of service, commitment and conformance which cover the different aspects of active information management, change control and security of supply. Because we care. As part of the Bormed" product portfolio, in case of notifiable change the grade can be made available up to 5 years (2 years pre-notification and last call volume with 3 years shelf life); subject to mutual agreement. Cas No. 9002-88-4

Typical characteristics:

  • No additives
  • Sterilization: EtO; radiation
  • Good flexibility
Applications: Bormed" LE6600-PH has been evaluated according to different regulations and standards. Typical applications are mentioned below for medical and diagnostic devices or pharmaceutical packaging. However, Borealis should be consulted for final approval to evaluate the use of Bormed" LE6600-PH.
  • Blow-fill-seal pharmaceutical packaging (e.g. bottles, ampoules)
  • Flexible pharmaceutical packaging (e.g. pouches for IV/CAPD)
  • Bottles for oral/topical drug administration
  • Packaging for pharmaceutical, medical device & diagnostic products

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ISO 1183-1/Method A
Melt Flow 1.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45.045.0ISO 868
Tensile Strength, Yield 13.0 MPa1890 psi50 mm/min; ISO 527-1
Elongation at Yield 85.0 %85.0 %50 mm/min; ISO 527-1
Tensile Modulus 0.170 GPa24.7 ksi1 mm/min; ISO 527-1
Flexural Modulus 0.170 GPa24.7 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 °C230 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C106 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 165 - 200 °C329 - 392 °F
Shelf Life 36.0 Month36.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9653 / 323010

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.